A copper and copper alloy liquid cooling plate and its preparation method

Nov 24, 2026

Leave a message

Copper and copper alloys occupy a core position in thermal management components in fields such as AI computing power, new energy vehicles, and aerospace due to their excellent thermal and electrical conductivity. Copper and copper alloy liquid cooling plates, as efficient heat dissipation components, their density, internal flow channel通畅ness, dimensional accuracy, surface quality, and residual stress levels directly determine the heat dissipation efficiency, assembly reliability, and long-term stability.

Laser additive manufacturing can achieve near-net-shape forming of complex structures. However, copper alloys have a low absorption rate for near-infrared laser and extremely high thermal conductivity. When forming copper and copper alloys using conventional process parameters (layer thickness of 0.03mm, scanning spacing of ~0.1mm), there are obvious challenges: 1) The powder layer thickness is large, and laser penetration is insufficient, resulting in interlayer non-fusion and low density; 2) The scanning spacing is too large, the fusion path overlap rate is only about 50%, and there are many inter-passage holes and gap defects, and gas pores are difficult to escape; 3) The thermal gradient is large, the internal stress is high, which easily causes cracks, deformation, and poor dimensional stability; 4) The step effect is significant, and the surface roughness is high; 5) The microstructure is relatively coarse, and the thermal and electrical conductivity cannot reach the optimal level; 6) The molten pool volume is large, the energy is concentrated, which easily causes a large amount of metal splashing, polluting the formed surface and blocking micro-flow channels.

Existing technologies mainly focus on optimizing parameters such as laser power and scanning speed, but have not systematically solved the integrated forming problem of copper and copper alloy high-density, high-precision thin-walled complex components.

This paper mainly achieves significant improvement in the bonding rate of the melt channels, effectively reduces internal defects such as interlayer non-melting and holes, refines the microstructure of the material, and reduces the step effect by setting the fixed printing layer thickness at 0.02mm, controlling the scanning interval within 0.04-0.07mm, and matching the appropriate laser process parameters. This method also fundamentally solves the technical problems such as poor stability of the molten pool, insufficient size accuracy, and surface roughness of copper and copper alloys caused by their high reflectivity and high thermal conductivity. By using this method, high-density, high-precision, thin-walled feature complete forming copper and copper alloy liquid cold plates with a thickness of 0.1-1.0mm and significantly reduced surface roughness Ra can be produced. This can greatly expand the application range of copper and copper alloys in high-end precision thermal control components.